Mechanical Properties Metric English Comments
Compressive Modulus 3.45 GPa
500 ksi
Mixed 2:1; TM R050-38
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive
Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature..
Compressive Modulus 3.45 GPa
500 ksi
TM R050-38
Resinlab® EP1285HD-16 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
Compressive Modulus 3.45 GPa
500 ksi
ASTM D695
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet)
Compressive Modulus 3.45 GPa
500 ksi
ASTM D695
Quadrant EPP Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet)
Compressive Modulus 3.45 GPa
500 ksi
ASTM D695
Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet)
Compressive Modulus 3.45 GPa

@Temperature 22.8 °C
500 ksi

@Temperature 73.0 °F
ASTM D695
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet)
This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis..
Compressive Modulus 3.45 GPa
500 ksi
Stabilized, typ, preliminary
Hexcel® HexWeb® CR III 1/16-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Compressive Modulus 3.45 GPa
500 ksi
ASTM D695
Ensinger Tecapeek® XP-103 Compression Molded PEEK Compound, 15% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Compressive Modulus 3.45 GPa
500 ksi
ASTM D695
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Compressive Modulus 3.45 GPa
500 ksi
ASTM D695
CIP Composites 100 Series Laminated Polymer Bearing Material
The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated..
Compressive Modulus 3.45 - 4.00 GPa
500 - 580 ksi
Average value: 3.72 GPa Grade Count:6
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Compressive Modulus 3.45 - 5.17 GPa
500 - 750 ksi
Average value: 4.41 GPa Grade Count:5
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..
Compressive Modulus 3.45 GPa

@Temperature 22.8 °C
500 ksi

@Temperature 73.0 °F
ASTM D695
Quadrant EPP Duratron® U2200 PEI Extruded 20% Glass Reinforced Polyetherimide
Compressive Modulus 3.45 GPa
500 ksi
ASTM D695
Quantum PEEK
Information provided by Quantum Advanced Engineering Plastics
Compressive Modulus 3.45 GPa
500 ksi
TM R050-38
Resinlab® EP1190 Flame Retardant Epoxy Casting Resin
Resinlab™ EP1190 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Proje..