Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 6.95 GPa @Strain 2.08 %, Temperature 0.000 °C |
1010 ksi @Strain 2.08 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Secant Modulus | 6.98 GPa @Strain 2.05 %, Temperature 0.000 °C |
1010 ksi @Strain 2.05 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject.. |
|||
Secant Modulus | 6.98 GPa @Strain 2.05 %, Temperature 0.000 °C |
1010 ksi @Strain 2.05 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in.. |
|||
Secant Modulus | 6.98 GPa @Strain 0.580 %, Temperature 23.0 °C |
1010 ksi @Strain 0.580 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Secant Modulus | 6.99 GPa @Strain 0.824 %, Temperature 0.000 °C |
1010 ksi @Strain 0.824 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Secant Modulus | 6.93 GPa @Strain 1.50 %, Temperature 0.000 °C |
1010 ksi @Strain 1.50 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |
|||
Secant Modulus | 6.99 GPa @Strain 1.53 %, Temperature -20.0 °C |
1010 ksi @Strain 1.53 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |
|||
Secant Modulus | 6.95 GPa @Strain 0.760 %, Temperature 0.000 °C |
1010 ksi @Strain 0.760 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |