Mechanical Properties Metric English Comments
Secant Modulus 1.47 GPa

@Strain 1.50 %,
Temperature 100 °C
213 ksi

@Strain 1.50 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Secant Modulus 1.47 GPa

@Strain 6.40 %,
Temperature -40.0 °C
213 ksi

@Strain 6.40 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr..
Secant Modulus 1.47 GPa

@Strain 4.99 %,
Temperature -20.0 °C
213 ksi

@Strain 4.99 %,
Temperature -4.00 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien..