Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.91 GPa @Strain 1.70 %, Temperature -40.0 °C |
422 ksi @Strain 1.70 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by.. |
|||
Secant Modulus | 2.91 GPa @Strain 3.80 %, Temperature 80.0 °C |
422 ksi @Strain 3.80 %, Temperature 176 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |