Polymer Property : Secant Modulus = 5.87 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 5.87 GPa

@Strain 1.20 %,
Temperature 100 °C
851 ksi

@Strain 1.20 %,
Temperature 212 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G15HSL NC010 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL NC010 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
Secant Modulus 5.87 GPa

@Strain 1.04 %,
Temperature 40.0 °C
851 ksi

@Strain 1.04 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm..