Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 6.32 GPa @Strain 0.700 %, Temperature 100 °C |
917 ksi @Strain 0.700 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G15HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL NC010 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Secant Modulus | 6.32 GPa @Strain 0.800 %, Temperature 100 °C |
917 ksi @Strain 0.800 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m.. |