Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 65.0 J @Load <=510 kg, Temperature 23.0 °C |
47.9 ft-lb @Load <=1120 lb, Temperature 73.4 °F |
ISO 6603-2 |
Lanxess Durethan® BC 550 Z DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Puncture Energy | 65.0 J @Temperature 0.000 °C |
47.9 ft-lb @Temperature 32.0 °F |
at Max load; ASTM D3763 |
Eastman Tritan TX1800 Copolyester Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo.. |
|||
Puncture Energy | 65.0 J @Temperature 0.000 °C |
47.9 ft-lb @Temperature 32.0 °F |
at Max load; ASTM D3763 |
Eastman Tritan TX1801 Copolyester, Natural Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo.. |
|||
Puncture Energy | 65.0 J @Temperature 0.000 °C |
47.9 ft-lb @Temperature 32.0 °F |
Energy @ Max. Load; ASTM D3763 |
Eastman Tritan WX500 Copolyester Eastman Tritan WX500 is a resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. This new-generati.. |
|||
Puncture Energy | 65.0 J @Temperature 0.000 °C |
47.9 ft-lb @Temperature 32.0 °F |
Energy @ Max. Load; ASTM D3763 |
Eastman Tritan WX510 Copolyester Eastman Tritan WX510 is a transparent blue resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. .. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2405 MAS048 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2607 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2652 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2665 MAS071 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2665 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2667 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2805 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Puncture Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ISO 6603-2 |
Covestro Makrolon® 3258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® FU1007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® Rx2435 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® ET2613 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® ET3127 Polycarbonate Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® ET3227 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® LED2643 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, .. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® LQ2647 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g.. |
|||
Puncture Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® Rx1851 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low.. |