Eastman Tritan TX1801 Copolyester, Natural

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Tritan
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Tritan TX1801 Copolyester, Natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGood heat resistanceOutstanding impact resistanceProduct Description:Eastman Tritan Copolyester TX1801 is an amorphous copolyester specifically developed for use in blow molding applications. Eastman Tritan Copolyester TX1801 contains a mold release derived from vegetable based sources. Its most outstanding features are excellent toughness, hydrolytic stability, heat resistance, and chemical resistance. In addition, this new generation copolyester offers excellent appearance and clarity. Eastman Tritan Copolyester TX1801 may be used in repeated use food contact articles under United States Food and Drug Administration (FDA) regulations.Information provided by Eastman.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength at Break 52.0 MPa
7540 psi
ASTM D638
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D638
Elongation at Break 139 %
139 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Tensile Modulus 1.609 GPa
233.4 ksi
ASTM D638
Flexural Strength 64.0 MPa
9280 psi
ASTM D790
Flexural Modulus 1.522 GPa
220.7 ksi
ASTM D790
Izod Impact, Notched 8.42 J/cm
15.8 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
Puncture Energy 62.0 J

@Temperature 23.0 °C
45.7 ft-lb

@Temperature 73.4 °F
at Max load; ASTM D3763
65.0 J

@Temperature 0.000 °C
47.9 ft-lb

@Temperature 32.0 °F
at Max load; ASTM D3763
67.0 J

@Temperature -40.0 °C
49.4 ft-lb

@Temperature -40.0 °F
at Max load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Transmission, Visible 91 %
91 %
Total; ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 235 - 255 °C
455 - 491 °F
EBM
260 - 280 °C
500 - 536 °F
ISBM
Mold Temperature 15.0 - 50.0 °C
59.0 - 122 °F
EBM
35.0 - 55.0 °C
95.0 - 131 °F
ISBM Blow Mold
40.0 - 65.0 °C
104 - 149 °F
ISBM Injection Mold
Drying Temperature 88.0 °C
190 °F
Dry Time 4 - 6 hour
4 - 6 hour