Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.00671 GPa | 0.973 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Non-Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00671 GPa | 0.973 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.25 PHR Thanecure ZM Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
200% Modulus | 0.00671 GPa | 0.973 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Non-Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00671 GPa | 0.973 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.25 PHR Thanecure ZM Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |