Mechanical Properties Metric English Comments
200% Modulus 0.00671 GPa
0.973 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Non-Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
200% Modulus 0.00671 GPa
0.973 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.25 PHR Thanecure ZM
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..
200% Modulus 0.00671 GPa
0.973 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Non-Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
200% Modulus 0.00671 GPa
0.973 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.25 PHR Thanecure ZM
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..