Polymer Property : Gardner Impact = 1.67 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 0.451 - 2.26 J
0.333 - 1.67 ft-lb
Average value: 1.13 J Grade Count:7
Overview of materials for Polypropylene with 30% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are..
Gardner Impact 0.300 - 2.26 J
0.221 - 1.67 ft-lb
Average value: 1.01 J Grade Count:8
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..