Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D5420 |
PolyOne OnForce™ LFT PP-60LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-FR2-[color]-EN Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Gardner Impact | >= 16.9 J | >= 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-FR3-[color]EN Modified PPO, UL 94 V-1 with HDT of 265 F, Extrusion Grade Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Gardner Impact | >= 16.9 J | >= 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP1-[color]EN Modified PPO, Extrusion Grade with HDT of 265 F Process: Extrusion Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP1-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Extrusion Notes: All physical, mechanical and thermal testing conduc.. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct.. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D3029 |
Polymer Resources TP-GP2 Polybutylene Terephthalate, General Purpose Polybutylene Terephthalate, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Gardner Impact | 16.9 J @Temperature -30.0 °C |
12.5 ft-lb @Temperature -22.0 °F |
Method G, geometry GC; ASTM D5420 |
Pinnacle Polymers 2150 H Medium Impact Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Gardner Impact | >= 16.9 J | >= 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP1 Modified PPO, General Purpose with HDT of 265 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | >= 16.9 J | >= 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP2 Modified PPO, General Purpose with HDT of 250 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | >= 16.9 J | >= 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP3 Modified PPO, General Purpose with HDT of 235 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 17.0 J @Temperature -30.0 °C |
12.5 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Flint Hills AP5520-HA Polypropylene Impact Copolymer Features: Nucleated, good processability, anti-stat and good mold release.Applications: Injection molding: large parts, containers, closuresInformation Provided by Flint Hills Resources |
|||
Gardner Impact | 17.0 J @Thickness 3.17 mm |
12.5 ft-lb @Thickness 0.125 in |
ASTM D3029 |
Ineos Styrenics Polystyrene 486N (NAFTA) High-impact grade of polystyrene with excellent ESCR.Information provided by BASF.Ineos Styrenics purchased this product line from BASF in 2005. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D 5420 |
Styrolution Zylar 650 MBS Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact.. |
|||
Gardner Impact | 17.0 J @Temperature -30.0 °C |
12.5 ft-lb @Temperature -22.0 °F |
|
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Gardner Impact | 17.0 J @Temperature -30.0 °C |
12.5 ft-lb @Temperature -22.0 °F |
|
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Gardner Impact | 17.0 J @Temperature -30.0 °C |
12.5 ft-lb @Temperature -22.0 °F |
|
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Gardner Impact | 17.0 J @Temperature -30.0 °C |
12.5 ft-lb @Temperature -22.0 °F |
|
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Gardner Impact | >= 16.9 J | >= 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | >= 16.9 J | >= 12.5 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP5 Modified PPO, General Purpose with HDT of 270 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 16.9 J | 12.5 ft-lb | ASTM D5420 |
RheTech Products HP508-01UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trim, Close out panelsConsolesInjection molding conditions reported in table.Information provided by RheTech Products. |