Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 3.05 J @Thickness 3.17 mm |
2.25 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite Optix® CA - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Gardner Impact | 3.05 J @Thickness 3.17 mm |
2.25 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite Optix® CP - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Gardner Impact | 3.05 J @Thickness 3.17 mm |
2.25 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite West Optix® CA - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Gardner Impact | 3.05 J @Thickness 3.17 mm |
2.25 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite West Optix® CP - 927 G High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Gardner Impact | 3.05 J @Thickness 3.17 mm |
2.25 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite West Optix® CP - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Gardner Impact | 3.05 J @Thickness 3.17 mm |
2.25 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite Optix® CP - 927 G High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Gardner Impact | 3.05 J | 2.25 ft-lb | Falling Weight; ASTM D3029GB |
Plaskolite West Optix® CA-927 G Clear Impact Modified Acrylic Resin Impact modified acrylic resin, injection molding gradeApplications: An impact-modified acrylic resin designed for medical or food uses. This resin offers impact strengths up to seven times of gener.. |
|||
Gardner Impact | 3.05 J | 2.25 ft-lb | Falling Weight; ASTM D3029GB |
Plaskolite West Optix® CA-927 G HF Clear Impact Modified Acrylic Resin Impact modified acrylic resin, injection molding gradeApplications: A high flow, impact-modified acrylic resin designed for medical or food uses. This resin offers impact strengths up to seven time.. |
|||
Gardner Impact | 3.05 - 7.34 J | 2.25 - 5.42 ft-lb | Average value: 5.20 J Grade Count:4 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |