Mechanical Properties Metric English Comments
Gardner Impact 3.05 - 7.34 J
2.25 - 5.42 ft-lb
Average value: 5.20 J Grade Count:4
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim..