Polymer Property : Gardner Impact = 2.95 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 4.00 - 4.00 J

@Temperature -29.0 - -29.0 °C
2.95 - 2.95 ft-lb

@Temperature -20.2 - -20.2 °F
Average value: 4.00 J Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..