Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 4.00 - 4.00 J @Temperature -29.0 - -29.0 °C |
2.95 - 2.95 ft-lb @Temperature -20.2 - -20.2 °F |
Average value: 4.00 J Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |