A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE , Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade
Manufacturer A. Schulman, Inc.
Trade Name POLYTROPE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains special heat stabilizers to allow usage in the under-hood environment. TPP 402 is only available in black compounds and is not UV stable.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Melt Index of Compound 0.60 g/10 min
0.60 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
ASTM D2240
Tensile Strength at Break 17.2 MPa
2500 psi
ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
Gardner Impact 36.0 J

@Temperature -30.0 °C
26.6 ft-lb

@Temperature -22.0 °F
Tear Strength 80.0 kN/m
456 pli
ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -45.0 °C
-49.0 °F