Material Notes:
Blowmoldable. DTUL 180F. UL rated.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D 792
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0060 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.0 MPa
6090 psi
Type I, 50 mm/min; ASTM D 638
Flexural Strength 59.0 MPa
8560 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2.24 GPa
325 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 2.67 J/cm

@Temperature 23.0 °C
5.00 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Gardner Impact 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
ASTM D 3029
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C

@Thickness 6.40 mm
180 °F

@Thickness 0.252 in
unannealed; ASTM D 648
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
UL RTI, Mechanical with Impact 50.0 °C
122 °F
UL 746B
UL RTI, Mechanical without Impact 50.0 °C
122 °F
UL 746B
Flammability, UL94 V-2

@Thickness 1.47 mm
V-2

@Thickness 0.0579 in
UL 94
V-1

@Thickness 2.99 mm
V-1

@Thickness 0.118 in
UL 94
5VA

@Thickness 3.81 mm
5VA

@Thickness 0.150 in
UL 94
Electrical Properties Metric English Comments
Arc Resistance 60 - 120 sec
60 - 120 sec
Tungsten, PLC code 6; ASTM D 495
Comparative Tracking Index 250 - 400 V
250 - 400 V
PLC code 2; UL 746A
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
PLC code 2; UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs
15 - 30 arcs
surface, PLC code 3; UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
>= 5.91 in/min
PLC code 4; UL 746A