Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 50.0 J @Temperature -20.0 °C |
36.9 ft-lb @Temperature -4.00 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 50.0 J @Temperature -20.0 °C |
36.9 ft-lb @Temperature -4.00 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 50.0 J @Temperature -20.0 °C |
36.9 ft-lb @Temperature -4.00 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® 700 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 50.0 J @Temperature -20.0 °C |
36.9 ft-lb @Temperature -4.00 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® 800 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can .. |
|||
Charpy Impact | 50.0 J @Temperature 0.000 °C |
36.9 ft-lb @Temperature 32.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® M 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 50.0 J @Temperature 0.000 °C |
36.9 ft-lb @Temperature 32.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® M 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 50.0 J @Temperature 0.000 °C |
36.9 ft-lb @Temperature 32.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® M 700 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 50.0 J @Temperature 0.000 °C |
36.9 ft-lb @Temperature 32.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® M 800 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can .. |
|||
Charpy Impact | 50.0 J @Temperature 0.000 °C |
36.9 ft-lb @Temperature 32.0 °F |
Longitudinal |
ThyssenKrupp XABO® 890 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Charpy Impact | 50.0 J @Temperature 0.000 °C |
36.9 ft-lb @Temperature 32.0 °F |
Longitudinal |
ThyssenKrupp XABO® 960 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Charpy Impact | 50.0 J @Temperature -30.0 °C |
36.9 ft-lb @Temperature -22.0 °F |
Longitudinal |
ThyssenKrupp XABO® 355 T Structural Steel This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Charpy Impact | 50.0 J @Temperature -30.0 °C |
36.9 ft-lb @Temperature -22.0 °F |
Longitudinal |
ThyssenKrupp XABO® 460 T Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |