Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 13100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 23.0 - 90.0 MPa
3340 - 13100 psi
Average value: 49.3 MPa Grade Count:31
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..