Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 165 - 200 MPa | 23900 - 29000 psi | Average value: 172 MPa Grade Count:3 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Ball Indentation Hardness | 108 - 200 MPa | 15700 - 29000 psi | Average value: 132 MPa Grade Count:4 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
Ball Indentation Hardness | 170 - 200 MPa @Time 30.0 sec |
24700 - 29000 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe PA 46 Nylon 46 PA 46 is primarily used in higher temperature ranges where stiffness, creep resistance, continuous heat stability and fatigue strength are required. Therefore PA 46 is suitable for high quality app.. |
|||
Ball Indentation Hardness | 70.0 - 200 MPa | 10200 - 29000 psi | Average value: 155 MPa Grade Count:31 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Ball Indentation Hardness | 150 - 200 MPa | 21800 - 29000 psi | Average value: 170 MPa Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |