Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 150 MPa | 21800 psi | dry; ISO 2039-1 |
Murtfeldt Murylon® B Nylon 6 Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO2039.1 DIN.53456 |
Omnia Plastica Akulon® POM h Acetal Homopolymer The general features of homopolymer acetalic resin are similar to those of copolymer POM c, except that service temperature (under load) is slightly higher but resistance to hydrolysis and strong al.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Nilit FRIANYL B63 KV25 Nylon 6 for injection molding, 25% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Nilit FRIANYL B63 SG-GV20 Nylon 6 for injection molding, 20% glass fiber reinforced Nylon 6 for injection molding, light impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Nilit FRIANYL A63 K Nylon 6.6 for injection molding Nylon 6.6 for injection molding, formulated for the coloration of button baths.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Nilit FRIANYL A63 V0 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Nilit FRIANYL B63 SG30 Nylon 6 for injection molding, 30% mineral filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039 |
GEHR Plastics Corzan® PVC-C Polyvinylchloride Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Lanxess Durethan® B 40 SK 000000 Nylon 6 PA 6, non-reinforced, injection molding |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg, Time 30.0 sec |
21800 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Polystyrol 158 K GR 2 PS Description: Polystyrol 158 K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blend s with high impact Polystyrol in heat contact applicati.. |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg, Time 30.0 sec |
21800 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Polystyrol 168 N GR 2 PS Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Styrolution PS 116 N/L GPPS Styrolution PS 116N/L is a general purpose polystyrene grade with excellent flow properties and improved heat resistance.Excellent flow propertiesHigh heat resistanceInformation provided by Styrolut.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Styrolution PS 147F GPPS Styrolution PS 147F is a highly transparent GPPS grade. It gives excellent mechanical and heat resistance properties while providing with easy processability and short cycle time.Medium FlowEasy pro.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Styrolution PS 153F GPPS Styrolution PS 153F is general purpose polystyrene with high heat resistance and good flow properties. Styrolution PS 153F is free of internal lubricants, e.g. zinc stearate.Free of internal lubrica.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics OPTAMID® Cast Polyamide 6, Dry Application: deflection rope sheaves for elevatorsInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg, Time 30.0 sec |
21800 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Polystyrol 165 H GR 21 PS Description: Polystyrol 165 H is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.Applications: In blends with high impact Polystyrene or Styrolux; thermo.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Styrolution PS 158K GPPS Styrolution PS 158K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact Styrolution PS in heat contact applications; fo.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® 1SBVX-30H LDS black PA1010-GF30 Product Description: Grilamid 1SBVX-30H LDS black is a 30% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSG-30/4 H black 9839 PA666-GF30 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4185 black 9453 PA* Product description: Grivory XE 4185 is a non-reinforced heat stabilized engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation: PA 10.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-50 PA6-GF50 Product description: Grilon BG-50 is a heat stabilized, normal viscosity PA6 injection molding grade with 50% glass fibers. Grilon BG-50 has the following important properties: High stiffnessGood su.. |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg, Time 30.0 sec |
21800 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® Z2320 003 POM Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | GB3398 |
Beijing Evergrow Resources Oilon Information provided by Beijing Evergrow Resources. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | H 358/30; Ø 50x4mm; ISO 2039-1 |
SYNTHOS Krasten® 171 General Purpose Polystyrene Very good heat resistance and mechanical strength. Examples of Application:Extrusion – biaxial-oriented sheets BOPS, XPS – lightweight insulating boards, shower enclosure panels, blends with high .. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | H 358/30; Ø 50x4mm; ISO 2039-1 |
SYNTHOS Krasten® 172 General Purpose Polystyrene Very good heat resistance and mechanical strength. Examples of Application:Extrusion – cups for hot drinks, shower enclosure panels, lightweight XPS sheets. Blends with high impact polystyrene, SBS.. |
|||
Ball Indentation Hardness | 150 - 200 MPa | 21800 - 29000 psi | Average value: 170 MPa Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |