Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 57.0 MPa | 8270 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 700 Ultra High Molecular Weight Polyethylene Application: wear liners, sliding platesInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 57.0 MPa | 8270 psi | H385/30; ISO 2039 |
Borealis Daplen™ KSR65T20 Polypropylene Compound 20% Mineral Filled Daplen KSR65T20 is a 20% mineral filled grade for injection molding. Daplen KSR65T20 has been developed especially for the car industry, to be used in interior parts. Daplen KSR65T20 offers very g.. |
|||
Ball Indentation Hardness | 57.0 - 60.0 MPa | 8270 - 8700 psi | ISO 2032-N132 |
Adamas Adalon® 814 PTFE, 55% Bronze, 5% MoS2 Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 57.0 - 60.0 MPa | 8270 - 8700 psi | ISO 2032-N132 |
Adamas Adalon® 817 PTFE, 60% Bronze Information provided by Adamas, HPM |