Mechanical Properties Metric English Comments
Ball Indentation Hardness 78.0 MPa
11300 psi
DIN 53456
Global PP-2340-S Polypropylene Block Copolymer
Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-electrical appliances, bases, panels, auto parts, cupsInformation provided by Global Polymers Corpo..
Ball Indentation Hardness 78.0 MPa
11300 psi
132 N/10s; ISO 2039
Borealis HK060AE Polypropylene Homopolymer
HK060AE is a special low viscosity polypropylene homopolymer compound developed to fit the production of glass matt reinforced thermoplastics. This material is also suitable as base resin for the pr..
Ball Indentation Hardness 78.0 MPa
11300 psi
358 N/30s; ISO 2039
Borealis PS65T20 Polypropylene Compound, Mineral Filled
PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applic..
Ball Indentation Hardness 78.0 MPa
11300 psi
H358/30; ISO 2039-1
Chi Mei Polylac® PA-764B ABS - Flame Retardant
F.R. Weather Resistant