Polymer Property : Ball Indentation Hardness = 9570 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 66.0 - 150 MPa
9570 - 21800 psi
Average value: 138 MPa Grade Count:13
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Ball Indentation Hardness 66.0 MPa
9570 psi
DIN 53456
Global PP-3240-H Polypropylene Random Copolymer
Description-medium stiffness, low melting temperatures, very good for seal Applications-sheets, bottlesInformation provided by Global Polymers Corporation.
Ball Indentation Hardness 66.0 MPa

@Load 36.5 kg,
Time 30.0 sec
9570 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Styrolution Polystyrol 486 M GR 2 PS
Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys..
Ball Indentation Hardness 66.0 MPa
9570 psi
ISO 2039-1
Styrolution PS 486N HIPS
Styrolution PS 486N is a normal flowing, high impact grade that is especially suitable for blends with a high proportion of general purpose polystyrene (preferably Styrolution PS 165N of Styrolution..
Ball Indentation Hardness 66.0 MPa
9570 psi
H 385/30; ISO 2039
Borealis Xmod™ PC75 High Crystalline Polypropylene Copolymer
Xmod PC75 is a HCPP intended for injection molding of automotive interior parts. Xmod PC75 is a very easy-flowing material combined with a good balance between impact strength and stiffness. The m..
Ball Indentation Hardness 66.0 MPa
9570 psi
H 385/30; ISO 2039
Borealis Xmod™ MC55T1 Polypropylene Compound 10% Mineral Filled
Xmod MC55t1 is a 10% mineral filled grade based on HCPP intended for injection molding. Xmod has been developed especially for the car industry, to be used in interior parts. XMod offers very good ..