Material Notes:
Styrolution PS 486N is a normal flowing, high impact grade that is especially suitable for blends with a high proportion of general purpose polystyrene (preferably Styrolution PS 165N of Styrolution PS 158N for better heat resistance). It is suitable for all kinds of thermoformed packaging.Suitable for blending with high proportions of GPPSUL 94 HBInformation provided by Styrolution
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Moisture Absorption at Equilibrium <= 0.10 %

@Temperature 23.0 °C
<= 0.10 %

@Temperature 73.4 °F
50% RH; ISO 62
Water Absorption at Saturation <= 0.10 %

@Temperature 23.0 °C
<= 0.10 %

@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ISO 294-4
Melt Flow 4.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Ball Indentation Hardness 66.0 MPa
9570 psi
ISO 2039-1
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527
Elongation at Break 35 %
35 %
ISO 527
Elongation at Yield 1.5 %
1.5 %
ISO 527
Tensile Modulus 1.80 GPa
261 ksi
ISO 527
Charpy Impact Unnotched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
165 °F
ISO 75
Vicat Softening Point 90.0 °C

@Load 5.10 kg
194 °F

@Load 11.2 lb
120°C/h; ASTM D 1525
96.0 °C

@Load 1.02 kg
205 °F

@Load 2.25 lb
50°C/h; ISO 306
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+18 ohm-cm
>= 1.00e+18 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
IEC 60093
Dielectric Constant 2.5

@Frequency 100 Hz
2.5

@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.00040

@Frequency 100 Hz
0.00040

@Frequency 100 Hz
IEC 60250
0.00040

@Frequency 1.00e+6 Hz
0.00040

@Frequency 1.00e+6 Hz
IEC 60250
Processing Properties Metric English Comments
Melt Temperature 180 - 260 °C
356 - 500 °F
ISO 294
Injection Velocity 200 mm/sec
7.87 in/sec
ISO 294