Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 224 MPa @Temperature 163 °C |
32500 psi @Temperature 325 °F |
Open Hole Compression; Wet |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber Information provided by HexCel |