Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.218 J/cm²
1.04 ft-lb/in²
ASTM D256
Plenco 00714 Melamine-Phenolic, Granular, Compression Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
Charpy Impact, Notched 0.218 J/cm²
1.04 ft-lb/in²
ASTM D256
Plenco 1501 Polyester, Pellet, Injection Molded
PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va..
Charpy Impact, Notched 0.218 J/cm²
1.04 ft-lb/in²
ASTM D256
Plenco 4414 Phenolic, Granular, Transfer Molded
PLENCO 04414 is a flock and mineral filled phenolic molding compound. It is formulated for use in electrical applications that require improved heat resistance, mechanical strength, and dimensional ..
Charpy Impact, Notched 0.218 J/cm²
1.04 ft-lb/in²
ASTM D256
Plenco 4466 Phenolic, Granular, Compression Molded
PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466..
Charpy Impact, Notched 0.218 J/cm²
1.04 ft-lb/in²
ASTM D256
Plenco 4304 Phenolic, Nodular, Injection Molded
PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component ..