Polymer Property : Charpy Impact, Notched = 15.0 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 3.15 J/cm²

@Temperature 22.8 °C
15.0 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Charpy Impact, Notched 3.15 J/cm²
15.0 ft-lb/in²
ISO 179/1EA-1993
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH50
Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal ..
Charpy Impact, Notched 3.15 J/cm²
15.0 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® C 216 V30 PA6, 30% glass fiber, Conditioned
Description: Polyamide PA6, reinforced with 30 % of glass fiber, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: It has good mechanical properties, it is used..
Charpy Impact, Notched 3.15 J/cm²
15.0 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, Conditioned
Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers..
Charpy Impact, Notched 3.15 J/cm²
15.0 ft-lb/in²
ISO 179/1eA
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, Conditioned
Description: TECHNYLSTARâ„¢ S 218 V30 is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is..