Solvay TECHNYL® C 216 V30 PA6, 30% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 216 V30 PA6, 30% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide PA6, reinforced with 30 % of glass fiber, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: It has good mechanical properties, it is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. It is used in the automotive industry and electrical sectors.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ISO 527 Type 1A
Elongation at Break 4.5 %
4.5 %
ISO 527 Type 1A
Tensile Modulus 6.20 GPa
899 ksi
ISO 527 Type 1A
Flexural Modulus 5.50 GPa
798 ksi
ISO 178
Izod Impact, Notched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 10.8 J/cm²
51.4 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 3.15 J/cm²
15.0 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Constant 4.5
4.5
IEC 60250
Dielectric Strength 22.0 kV/mm
559 kV/in
IEC 60243
Dissipation Factor 0.090
0.090
IEC 60250
Comparative Tracking Index 475 V
475 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Users viewing this material also viewed the following: