Mechanical Properties Metric English Comments
Charpy Impact, Notched 18.0 J/cm²
85.7 ft-lb/in²
Partial Break; ISO 179-1/1eA
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data)
Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan..
Charpy Impact, Notched >= 18.0 J/cm²
>= 85.7 ft-lb/in²
Requirement
Westlake Plastics Lennite® GUR1020 (Type I) Ultra-high Molecular Weight Polyethylene For Medical Applications
Medical grade Lennite UHMWPE is produced from premium resins in accordance with ASTM specification F648 and International Standard ISO 5834-1 for surgical implants. Westlake Plastics' proprietary m..
Charpy Impact, Notched 18.0 J/cm²

@Temperature -20.0 °C
85.7 ft-lb/in²

@Temperature -4.00 °F
After conditioning at 23°C/50%RH; ISO 179/Af
Arkema Group Orgalloy® RS 6630 Polyamide 6.6 Alloy 30% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group
Charpy Impact, Notched 18.0 J/cm²
85.7 ft-lb/in²
Longitudinal direction; ISO 179/2fn
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix
AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This..
Charpy Impact, Notched >= 18.0 J/cm²
>= 85.7 ft-lb/in²
Determined with double-notched specimens; ISO 11542-2
Braskem UTEC® 3041 Ultra High Molecular Weight Polyethylene
Applications which require high impact resistance and use of pigments and/or additives - filters, technical and porous parts, compression molded sheets.Information provided by Braskem.
Charpy Impact, Notched 18.0 J/cm²

@Temperature -20.0 °C
85.7 ft-lb/in²

@Temperature -4.00 °F
Dry; ISO 179/Af
Arkema Group Orgalloy® RS 6030 Polyamide 6 Alloy 30% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6 basedMolding of Engineering PartsInformation provided by Arkema Group