Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO179/3C DIN.53453 |
Omnia Plastica Omniamid PA6 G - G - at 50% RH Cast nylon 6. The method of production of this polyamide (i.e. the polymerisation of the caprolactam directly in the mould) allows the production of stock shapes in larger than normal dimensions, su.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO179/3C DIN.53453 |
Omnia Plastica Omniamid PA6 GHR - HR - at 50% RH Cast nylon 6 produced with the addition of graphite and a special lubricator which gives to this product better properties than natural PA6G. Whilst retaining the general features of OMNIAMID G it i.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO179/3C DIN.53453 |
Omnia Plastica PC Polycarbonate This amorphous polymer is commonly used for its high shock resistance even at low temperature. It is not a material recommended for mechanical applications, even if its dimensional stability does ma.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® HMG94MD ABS Superior flow, injection molding ABS for medical applications. Good impact. For thin-wall applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 S20 Nylon 6 for injection molding Nylon 6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
Iran Petrochemical (PCC) EX 2 S HF 7750 M2 High Density Polyethylene EX2S is a high density polyethylene with 1-Butene as co monomer. It is medium molar mass, low density grade with a narrow molar mass distribution, high rigidity, good tear strength. Applications: .. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene EX3-80 is a high density polyethylene with 1-Butene as co monomer. It is natural, good ESCR, good impact strength, tough and rigid pipe resin. Applications: pipe extrusion PE 80 class, industrial a.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | 80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics Valox® V8030CS PBT+PET Glass filled Valox with enhanced surface |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
Borealis Nepol™ GB303HP 30% Long Glass Fiber Reinforced Polypropylene Nepol GB303HP is a 30% long glass fiber reinforced polypropylene grade, produced using Borealis ` propriety and exclusive, patented Nepol technology intended for injection molding and extrusion. Th.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Bayer Test |
Covestro Baydur® 730 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Charpy Impact, Notched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GV 20 HWCP 20% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 100T BK602 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T BK602 is a toughened high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed parts where o.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) 43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179 |
Chi Mei Polylac® PA-727 ABS Electro-plating |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® LE60 THM Polyamide Alloy Polyamide Alloy, Semi-Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.30 J/cm² @Temperature -20.0 °C |
10.9 ft-lb/in² @Temperature -4.00 °F |
Dry; ISO 179/Af |
Arkema Group Orgalloy® RS 60E10 Polyamide Alloy Polyamide Alloy, Rigid Blown film gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Conditioned, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact, Notched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Conditioned, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179 |
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat
cushion .. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |