Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.490 J/cm²
2.33 ft-lb/in²
ISO 179/1eA
Radici Radilon® AHS (dry) Nylon 66
General purposeInformation provided by Radici group.
Charpy Impact, Notched 0.490 J/cm²
2.33 ft-lb/in²
Eastman Eastapak 7352 PET  (discontinued **)
Unreinforced Low IV. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003.
Charpy Impact, Notched 0.490 J/cm²

@Temperature -30.0 °C
2.33 ft-lb/in²

@Temperature -22.0 °F
Eastman Tenite 105-33 Cellulose Acetate  (discontinued **)
33% Plasticized ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 0.490 J/cm²
2.33 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 800FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, Super High Viscosity
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.490 J/cm²
2.33 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® CN5315 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.490 J/cm²

@Temperature -30.0 °C
2.33 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Dry)
Designation ISO 1874-PA12,EHLS,22-010,MD05Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Low friction coefficient. No need of l..
Charpy Impact, Notched 0.490 J/cm²

@Temperature -30.0 °C
2.33 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® MB 3945 Nylon 11, Rotomolding Grade (Dry)
Designation ISO 1874-PA11-P,RDR,12-004Semi-rigid grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyeth..
Charpy Impact, Notched 0.490 J/cm²
2.33 ft-lb/in²
ISO 179
BASF Ultramid® 1310-11 NF2001 PA66 (Dry)
Ultramid 1310-11 NF2001 is a controlled crystallization, fast cycling PA6/6 which provides extremely fast cycle times and improved productivity over Ultramid 1000.
Charpy Impact, Notched 0.490 J/cm²
2.33 ft-lb/in²
Arkema Group Rilsan® MB 3000 Nylon 11, Sheathing Grade (Conditioned)
Designation ISO 1874-PA11,MF,12-010Polyvalent rigid grade for injection molding and sheathing of cables. Available color: natural. Flame retardant agent, halogen free. Fire-resistant. Easy to be pro..
Charpy Impact, Notched 0.490 - 2.42 J/cm²

@Temperature -30.0 - -30.0 °C
2.33 - 11.5 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.17 J/cm² Grade Count:18