Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Eastapak 7352 PET  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastapak 7352 PET  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unreinforced Low IV. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.0 MPa
8270 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Elongation at Yield 3.8 %
3.8 %
Tensile Modulus 2.60 GPa
377 ksi
1mm/min
Charpy Impact Unnotched NB
NB
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched 0.490 J/cm²
2.33 ft-lb/in²
0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 77.0 µm/m-°C

@Temperature 20.0 °C
42.8 µin/in-°F

@Temperature 68.0 °F
CTE, linear, Transverse to Flow 48.0 µm/m-°C

@Temperature 20.0 °C
26.7 µin/in-°F

@Temperature 68.0 °F
Melting Point 250 °C
482 °F
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
Vicat Softening Point 74.0 °C
165 °F
Glass Transition Temp, Tg 77.0 °C
171 °F
Processing Properties Metric English Comments
Melt Temperature 270 - 290 °C
518 - 554 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved