Polymer Property : Charpy Impact, Notched = 3.71 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.780 J/cm²

@Temperature -30.0 °C
3.71 ft-lb/in²

@Temperature -22.0 °F
Eastman Tenite 383A-10 Cellulose Acetate Propionate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 0.780 J/cm²
3.71 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® ST45G6 Toughened Acrylic Polymer
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b..
Charpy Impact, Notched 0.780 J/cm²
3.71 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® AR 218 V33 Black 34 N Nylon 66, 33% glass fiber, DRY
Description: Polyamide 66, reinforced with 33% of glass fiber, containing recycled material, for injection molding, specially stabilized to improve its resistance to automotive cooling liquids.Avail..
Charpy Impact, Notched 0.780 J/cm²
3.71 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 733LD Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.780 J/cm²
3.71 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® C5330 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.780 J/cm²

@Temperature -30.0 °C
3.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..
Charpy Impact, Notched 0.780 J/cm²

@Temperature -30.0 °C
3.71 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Pebax® 7233 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 72 shore D Highest modulus PEBAX Applications: medical, extrusion SportISO data provided by the manufacturer, Arkema.
Charpy Impact, Notched >= 0.780 J/cm²

@Temperature 23.0 °C
>= 3.71 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
AKG Polymers Vision PP PPC BL1008 Polypropylene Copolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Charpy Impact, Notched 0.780 J/cm²
3.71 ft-lb/in²
ISO 179/1eA
Cathay PA513 Renewable Engineering Polyamide
Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr..
Charpy Impact, Notched 0.780 J/cm²

@Temperature 23.0 °C
3.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
BASF Ultradur® S 4090 G6X High Speed 30% Glass Filled PBT
Description: Low-warpage, easy-flowing injection molding grade with 30 % glass fibers for technical parts, for which dimensional stability is very important, reduction of wall thickness (eg, e/e hou..