Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.10 - 7.00 J/cm²

@Temperature -40.0 - -30.0 °C
5.24 - 33.3 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 2.14 J/cm² Grade Count:11
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Charpy Impact, Notched 3.00 - 7.00 J/cm²
14.3 - 33.3 ft-lb/in²
Average value: 5.50 J/cm² Grade Count:6
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 0.300 - 7.00 J/cm²
1.43 - 33.3 ft-lb/in²
Average value: 2.60 J/cm² Grade Count:3
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
Charpy Impact, Notched 0.300 - 7.00 J/cm²

@Temperature -30.0 - -30.0 °C
1.43 - 33.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 2.82 J/cm² Grade Count:4
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Charpy Impact, Notched 3.00 - 7.00 J/cm²
14.3 - 33.3 ft-lb/in²
Average value: 4.84 J/cm² Grade Count:16
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi..
Charpy Impact, Notched 0.150 - 7.00 J/cm²
0.714 - 33.3 ft-lb/in²
Average value: 1.46 J/cm² Grade Count:100
Overview of materials for Polypropylene, Mineral Reinforced