Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.06 - 1.30 J/cm² @Temperature -30.0 - 30.0 °C |
5.04 - 6.19 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 1.14 J/cm² Grade Count:3 |
Overview of materials for Nylon 12, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Charpy Impact, Notched | 1.06 J/cm² @Temperature 23.0 °C |
5.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BFG30-BN00B2 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 1.06 J/cm² | 5.04 ft-lb/in² | |
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Dry) Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas.. |
|||
Charpy Impact, Notched | 1.06 J/cm² @Temperature -30.0 °C |
5.04 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Charpy Impact, Notched | 1.06 J/cm² @Temperature -30.0 °C |
5.04 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BECN TL Nylon 11, Sheathing Grade (Conditioned) Designation ISO 1874-PA11,KHL,12-010Rigid grade for sheathing of wires and cables. Available color: natural. Light and heat stabilized.High abrasion resistance. Well adapted melt viscosity. Ability .. |
|||
Charpy Impact, Notched | 1.06 J/cm² @Temperature -30.0 °C |
5.04 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BMN D Nylon 11 (Conditioned) Designation ISO 1874-PA11,MR,12-010Rigid grade for injection molding. Available colors: black, blue, natural, orange, white. Mold release agent.High mechanical properties. Easy filling of the mold d.. |
|||
Charpy Impact, Notched | 1.06 J/cm² | 5.04 ft-lb/in² | |
Arkema Group Rilsan® BZM 8 NOIR TL Nylon 11, 8% Glass Fiber Filled (Dry) Designation ISO 1874-PA11,MHL,18-020,GF8Rigid grade with glass fiber (8%) filler for injection molding. Available color: black. Light and heat stabilized.Rigidity. Outstanding compromise between goo.. |
|||
Charpy Impact, Notched | 1.06 J/cm² @Temperature -30.0 °C |
5.04 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |