Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.26 J/cm²

@Temperature 22.8 °C
6.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-FR6 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 300F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Charpy Impact, Notched 1.26 J/cm²
6.00 ft-lb/in²
Eastman Tenite 264-10 CAB Cellulose Acetate Butyrate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 1.26 - 1.40 J/cm²
6.00 - 6.66 ft-lb/in²
Average value: 1.31 J/cm² Grade Count:3
Overview of materials for Nylon 12, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Charpy Impact, Notched 1.26 J/cm²
6.00 ft-lb/in²
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..
Charpy Impact, Notched 1.26 - 2.12 J/cm²
6.00 - 10.1 ft-lb/in²
Average value: 1.61 J/cm² Grade Count:3
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..