Polymer Property : Izod Impact, Notched = 0.187 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.100 - 0.150 J/cm
0.187 - 0.281 ft-lb/in
ASTM D256
Prodways PLASTCure Model 200 3D Printing Polymer
High temperature resistance.Thermoforming applicationsInformation provided by Genistar.
Izod Impact, Notched 0.100 J/cm
0.187 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.
Izod Impact, Notched 0.100 J/cm

@Temperature 23.0 °C
0.187 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® OQ1060 PC Copolymer
Optical quality, high flow, high purity Polycarbonate copolymer resin with reduced oxygen transmission for advanced DVD applications such as Limited Play DVD.This data was supplied by SABIC-IP for t..
Izod Impact, Notched 0.100 J/cm
0.187 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP KONDUIT MT00E PP
LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing 70% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Izod Impact, Notched 0.100 J/cm
0.187 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Asia Pacific)
LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Izod Impact, Notched 0.100 J/cm
0.187 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Europe-Africa-Middle East)
LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Izod Impact, Notched 0.100 J/cm
0.187 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP CBL36XXC PS (Asia Pacific)
LNP* Lubricomp* CBL36XXC is a compound based on Polystyrene resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Notched 0.100 J/cm
0.187 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Asia Pacific)
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.
Izod Impact, Notched 0.100 J/cm

@Temperature 23.0 °C
0.187 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg..
Izod Impact, Notched 0.100 - 4.48 J/cm
0.187 - 8.40 ft-lb/in
Average value: 1.87 J/cm Grade Count:125
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Izod Impact, Notched 0.100 J/cm
0.187 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP CBL36XXC PS
LNP* LUBRICOMP* CBL36XXC is a compound based on Polystyrene resin containing 30% Glass Bead and 15% PTFE. Added features of this material include: Wear Resistant.
Izod Impact, Notched 0.100 J/cm

@Temperature 23.0 °C
0.187 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Lubricomp CI001 PS
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the America..
Izod Impact, Notched 0.100 J/cm

@Temperature 23.0 °C
0.187 ft-lb/in

@Temperature 73.4 °F
ISO 180/A
Cossa Polimeri ESTABLEND PA 4016 GF ABS / Nylon 6 Blend, 8% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedExceptional chemical resistance, excellent heat resistance, good dimensional stabilityInformation ..
Izod Impact, Notched 0.100 J/cm

@Temperature 23.0 °C
0.187 ft-lb/in

@Temperature 73.4 °F
ISO 180/A
Cossa Polimeri ESTABLEND PA 1030 GF HI ABS / Nylon 6 Blend, 15% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.15% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi..
Izod Impact, Notched 0.100 J/cm

@Temperature 23.0 °C
0.187 ft-lb/in

@Temperature 73.4 °F
ISO 180/A
Cossa Polimeri ESTABLEND PA 1040 GF HI ABS / Nylon 6 Blend, 20% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.20% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi..
Izod Impact, Notched 0.100 J/cm

@Temperature 23.0 °C
0.187 ft-lb/in

@Temperature 73.4 °F
ISO 180/A
Cossa Polimeri ESTABLEND PA 1050 GF HI ABS / Nylon 6 Blend, 25% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.25% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi..
Izod Impact, Notched 0.100 J/cm

@Temperature 23.0 °C
0.187 ft-lb/in

@Temperature 73.4 °F
ISO 180/A
Cossa Polimeri ESTABLEND PA 1424 GF HI ABS / Nylon 6 Blend, 12% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.12% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi..
Izod Impact, Notched 0.100 J/cm

@Temperature 23.0 °C
0.187 ft-lb/in

@Temperature 73.4 °F
ISO 180/A
Cossa Polimeri ESTABLEND PA 1616 GF ABS / Nylon 6 Blend, 8% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, good dimensional stabil..
Izod Impact, Notched 0.100 J/cm

@Thickness 3.20 mm
0.187 ft-lb/in

@Thickness 0.126 in
ASTM D256
Beijing Chemical Industry KAIFA® GL3100 ABS Flame-Retardant Grade
Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group)
Izod Impact, Notched 0.100 J/cm

@Temperature 23.0 °C
0.187 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific)
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa..
Izod Impact, Notched 0.100 - 6.40 J/cm
0.187 - 12.0 ft-lb/in
Average value: 2.22 J/cm Grade Count:309
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Izod Impact, Notched 0.100 J/cm
0.187 ft-lb/in
63.5*12.7*3.2mm, Cut; ASTM D256
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1040 PP
SABIC® PPcompound 15T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound, suitable for injection molding applications. The IMDS ID is 16487994
Izod Impact, Notched 0.100 J/cm

@Temperature 23.0 °C
0.187 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LATI LATILUB 80-40GRT Polyphenylene sulfide Base (PPS), 40% Graphite and PTFE Self Lubricating Plastic  (U
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..