Material Notes:
LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing 70% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Physical Properties Metric English Comments
Density 1.94 g/cc
0.0701 lb/in³
ISO 1183
1.952 g/cc
0.07052 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0090 cm/cm

@Time 86400 sec
0.0090 in/in

@Time 24.0 hour
ASTM D955
0.0095 cm/cm

@Time 86400 sec
0.0095 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D955
0.0074 cm/cm

@Time 86400 sec
0.0074 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.0 MPa
3190 psi
ASTM D638
22.0 MPa
3190 psi
ISO 527
Elongation at Break 0.90 %
0.90 %
ISO 527
1.0 %
1.0 %
ASTM D638
Tensile Modulus 8.65 GPa
1250 ksi
1 mm/min; ISO 527
9.075 GPa
1316 ksi
50 mm/min; ASTM D638
Flexural Strength 44.0 MPa
6380 psi
ASTM D790
44.0 MPa
6380 psi
ISO 178
Flexural Modulus 8.16 GPa
1180 ksi
ISO 178
Izod Impact, Notched 0.100 J/cm
0.187 ft-lb/in
ASTM D256
Izod Impact, Unnotched 0.740 J/cm
1.39 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.43
0.43
ASTM D3702 Modified
Coefficient of Friction, Static 0.48
0.48
ASTM D3702 Modified
K (wear) Factor 2278 x 10-8 mm³/N-M
1131 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
ASTM E 1530
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
279 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
217 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af