Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.196133 - 0.85424 J/cm

@Temperature -30.0 - -18.0 °C
0.367438 - 1.6003 ft-lb/in

@Temperature -22.0 - -0.400 °F
Average value: 0.562 J/cm Grade Count:9
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched 0.196133 - 0.85424 J/cm

@Thickness 3.17 - 6.50 mm
0.367438 - 1.6003 ft-lb/in

@Thickness 0.125 - 0.256 in
Average value: 0.562 J/cm Grade Count:9
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched 0.196133 - 1.07 J/cm

@Temperature -30.0 - -30.0 °C
0.367438 - 2.00 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.377 J/cm Grade Count:11
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Izod Impact, Notched 0.196133 - 1.07 J/cm

@Thickness 3.17 - 6.40 mm
0.367438 - 2.00 ft-lb/in

@Thickness 0.125 - 0.252 in
Average value: 0.377 J/cm Grade Count:11
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Izod Impact, Notched 0.196133 - 0.220 J/cm

@Temperature -30.0 - -10.0 °C
0.367438 - 0.412 ft-lb/in

@Temperature -22.0 - 14.0 °F
Average value: 0.495 J/cm Grade Count:10
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.196133 - 0.220 J/cm

@Thickness 3.20 - 6.40 mm
0.367438 - 0.412 ft-lb/in

@Thickness 0.126 - 0.252 in
Average value: 0.495 J/cm Grade Count:10
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..