Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.534 - 1.07 J/cm | 1.00 - 2.00 ft-lb/in | |
PolyChem Alloy PolyOxyter 2501 PolyOxyter, an additive masterbatch product, has been specially formulated with reactive compounds to provide performance enhancement and processing improvement for Polyesters, Nylons, and Polycarbo.. |
|||
Izod Impact, Notched | 0.534 - 1.07 J/cm | 1.00 - 2.00 ft-lb/in | |
PolyChem Alloy PolyOxyter 5001 PolyOxyter, an additive masterbatch product, has been specially formulated with reactive compounds to provide performance enhancement and processing improvement for Polyesters, Nylons, and Polycarbo.. |
|||
Izod Impact, Notched | 0.214 - 1.07 J/cm | 0.400 - 2.00 ft-lb/in | Average value: 0.492 J/cm Grade Count:21 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Izod Impact, Notched | 0.235 - 1.07 J/cm | 0.440 - 2.00 ft-lb/in | Average value: 0.689 J/cm Grade Count:78 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Izod Impact, Notched | 0.235 - 1.07 J/cm | 0.440 - 2.00 ft-lb/in | Average value: 0.641 J/cm Grade Count:22 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.534 - 1.07 J/cm | 1.00 - 2.00 ft-lb/in | Average value: 0.749 J/cm Grade Count:9 |
Overview of materials for PEKK, Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Notched | 0.800 - 1.07 J/cm @Thickness 6.35 mm |
1.50 - 2.00 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ SY-000/05T High Impact Styrene - 5% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 1.01 - 1.07 J/cm @Temperature -20.0 - -20.0 °C |
1.89 - 2.00 ft-lb/in @Temperature -4.00 - -4.00 °F |
Average value: 0.864 J/cm Grade Count:2 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Izod Impact, Notched | 1.01 - 1.07 J/cm @Thickness 3.18 - 3.18 mm |
1.89 - 2.00 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 0.864 J/cm Grade Count:2 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Izod Impact, Notched | 0.534 - 1.07 J/cm | 1.00 - 2.00 ft-lb/in | Average value: 0.839 J/cm Grade Count:7 |
Overview of materials for Polycarbonate/Polysulfone Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched | 0.534 - 1.07 J/cm @Temperature 0.000 - 0.000 °C |
1.00 - 2.00 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.668 J/cm Grade Count:4 |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Notched | 0.534 - 1.07 J/cm @Thickness 3.18 - 3.18 mm |
1.00 - 2.00 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 0.668 J/cm Grade Count:4 |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Notched | 0.534 - 1.07 J/cm | 1.00 - 2.00 ft-lb/in | Average value: 0.835 J/cm Grade Count:19 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Izod Impact, Notched | 0.961 - 1.07 J/cm | 1.80 - 2.00 ft-lb/in | Average value: 1.00 J/cm Grade Count:5 |
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Izod Impact, Notched | 0.801 - 1.07 J/cm | 1.50 - 2.00 ft-lb/in | Average value: 0.921 J/cm Grade Count:4 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 0.196133 - 1.07 J/cm @Temperature -30.0 - -30.0 °C |
0.367438 - 2.00 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 0.377 J/cm Grade Count:11 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Izod Impact, Notched | 0.196133 - 1.07 J/cm @Thickness 3.17 - 6.40 mm |
0.367438 - 2.00 ft-lb/in @Thickness 0.125 - 0.252 in |
Average value: 0.377 J/cm Grade Count:11 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Izod Impact, Notched | 0.374 - 1.07 J/cm | 0.700 - 2.00 ft-lb/in | Average value: 0.807 J/cm Grade Count:10 |
Overview of materials for Nylon 66, Mineral Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Notched | 0.320 - 1.07 J/cm | 0.599 - 2.00 ft-lb/in | Average value: 0.505 J/cm Grade Count:13 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Notched | 0.427 - 1.07 J/cm | 0.800 - 2.00 ft-lb/in | Average value: 0.532 J/cm Grade Count:15 |
Overview of materials for Nylon 612 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Notched | 0.534 - 1.07 J/cm | 1.00 - 2.00 ft-lb/in | Average value: 0.849 J/cm Grade Count:10 |
Overview of materials for Nylon 11 with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ.. |
|||
Izod Impact, Notched | 0.667 - 1.07 J/cm | 1.25 - 2.00 ft-lb/in | ASTM D256 |
Buckeye Polymers BP RPPC 1020 TU BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Izod Impact, Notched | 0.534 - 1.07 J/cm | 1.00 - 2.00 ft-lb/in | |
Bulk Molding Compounds BMC 1401 Encapsulating Material, Electrical Grade BMC 1401 is an electrical grade of encapsulating material characterized by a balance of soft flow and cure rate to ensure complete and proper encapsulation without voiding. Generally too soft for co.. |
|||
Izod Impact, Notched | 0.270 - 1.07 J/cm | 0.506 - 2.00 ft-lb/in | Average value: 0.534 J/cm Grade Count:27 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched | 0.641 - 1.07 J/cm | 1.20 - 2.00 ft-lb/in | Average value: 0.822 J/cm Grade Count:18 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Izod Impact, Notched | 0.270 - 1.07 J/cm | 0.506 - 2.00 ft-lb/in | Average value: 0.616 J/cm Grade Count:41 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Izod Impact, Notched | 0.801 - 1.07 J/cm | 1.50 - 2.00 ft-lb/in | ASTM D256 |
Aaron Industries AAROLENE® ARPS HI 100-3 Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Izod Impact, Notched | 0.534 - 1.07 J/cm | 1.00 - 2.00 ft-lb/in | Average value: 0.714 J/cm Grade Count:11 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Izod Impact, Notched | 0.534 - 1.07 J/cm | 1.00 - 2.00 ft-lb/in | Average value: 0.641 J/cm Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 0.214 - 1.07 J/cm | 0.400 - 2.00 ft-lb/in | Average value: 0.442 J/cm Grade Count:24 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |