Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos H20Z-03 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H20Z-03 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a homopolymer containing nucleation and antistatic. It is designed for injection molding and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsGeneral purpose injection moldingConsumer productsRigid packagingBenefitsImproved processabilityGood mold releaseReduced cycle timeInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Density 0.904 - 0.908 g/cc
0.0327 - 0.0328 lb/in³
ASTM D1505
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 68 - 108
68 - 108
ASTM D785
Tensile Strength, Yield 37.8 MPa

@Temperature 23.0 °C
5480 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Yield 6.2 %
6.2 %
ASTM D638
Flexural Modulus 1.52 GPa

@Temperature 23.0 °C
220 ksi

@Temperature 73.4 °F
ASTM D790A
Izod Impact, Notched 0.187 - 0.320 J/cm

@Temperature 23.0 °C
0.350 - 0.600 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 126 °C
258 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved