Polymer Property : Izod Impact, Notched = 0.48051 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.48051 - 0.48051 J/cm

@Temperature -28.9 - -28.9 °C
0.90019 - 0.90019 ft-lb/in

@Temperature -20.0 - -20.0 °F
Average value: 0.481 J/cm Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Izod Impact, Notched 0.48051 - 2.40255 J/cm

@Temperature -40.0 - 0.000 °C
0.90019 - 4.50096 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 1.52 J/cm Grade Count:10
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Izod Impact, Notched 0.48051 - 2.40255 J/cm

@Thickness 3.17 - 3.20 mm
0.90019 - 4.50096 ft-lb/in

@Thickness 0.125 - 0.126 in
Average value: 1.52 J/cm Grade Count:10
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..