Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.497 J/cm @Thickness 3.17 mm |
0.930 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Polyram PB330I8 Nylon 6, 40% Mineral/Glass Filled Heat Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 0.497 J/cm | 0.930 ft-lb/in | ASTM D256A |
ExxonMobil PP6262 Polypropylene Homopolymer Product Description: A clarified homopolymer resin designed for production of extruded sheet and thermoformed containers. It exhibits excellent processing characteristics even in deep drawn applica.. |