Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | Low Temp |
Kolon KOPEL® KP3372 General Purpose TPE Resin KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very.. |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | DIN 53453; ASTM D256 |
Kolon NOPLA® KE831 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP1000H PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® HI2152 PBT+GF15% Description: Injection Molding, PBT+GF15%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® SG5200 PBT+PET+GF20% Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
Izod Impact, Notched | 0.539 J/cm @Temperature 23.0 °C |
1.01 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC R1610 Polypropylene Random Copolymer Features: SEETEC R1610 is a highly transparent ethylene-propylene random copolymer for injection molding applications. SEETEC R1610 exhibits an excellent transparency and a good impact strength. SEE.. |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® PM655 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Izod Impact, Notched | >= 0.539 J/cm @Thickness 6.35 mm |
>= 1.01 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 1100-211H Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP2156FT PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant, High FlowApplication: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.539 J/cm @Thickness 6.35 mm |
>= 1.01 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 2100-104B Product Description: PBT unreinforced flame-retarded injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellen.. |
|||
Izod Impact, Notched | >= 0.539 J/cm @Thickness 6.35 mm |
>= 1.01 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 3020-104 15% Glass Fiber Filled Product Description: A glass fiber 20% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Izod Impact, Notched | 0.539 J/cm @Temperature 23.0 °C |
1.01 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Polene 1111NX GA6 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 30% GLASS FIBRE REINFORCED HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, HIGH STIFFNESS LOW SHRINKAGEAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, .. |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® E202G15 PBT, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® E202G15 PBT, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | |
Zylog Hipolyene® 9011 UHF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N6C2 Nylon 6, 20% Mineral Reinforced |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
Cheng Yu Plastic NGCV2 Flame Retardant Nylon 6, 20% Mineral Reinforced |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TA210MS MoS2 Filled PA66 Resin Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,.. |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0334W10L1 Wollastonite Reinforced |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FRCV200 Flame Retardant Nylon 66, 30% Mineral Reinforced |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® CFPP 2040 Calcium Carbonate Filled Polypropylene AAROPRENE® CFPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Izod Impact, Notched | >= 0.539 J/cm @Thickness 6.35 mm |
>= 1.01 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 4115-201D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
E-Polymers TEKAPPO® JF101 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |