Polymer Property : Izod Impact, Notched = 0.569 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.304 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
0.569 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical Lupox® SG3180S PBT+PET+MF18%
Description: Injection Molding, PBT+PET+MF18%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical
Izod Impact, Notched 0.304 J/cm

@Temperature 23.0 °C
0.569 ft-lb/in

@Temperature 73.4 °F
ASTM D256
IRPC Polimaxx Polene 1111NX BA4 Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 20% BARIUM SULPHATE REINFORCED HIGH GLOSS APPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES
Izod Impact, Notched 0.304 J/cm
0.569 ft-lb/in
ASTM D256
E-Polymers SEPAZ® N2020L Nanoclay 2% High flow Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..
Izod Impact, Notched >= 0.304 J/cm
>= 0.569 ft-lb/in
ASTM D256
Gromax Evasin EV-3201V Ethylene-Vinyl Alcohol Copolymer
Unmodified random Co-Polymer of [Ethylene-Vinyl alcohol], designed for therm-plastic processing into Sheets and Foils with high Oxygen and Aroma Barrier EffectInformation provided by Gromax Enterpri..