IRPC Polimaxx Polene 1111NX BA4 Polypropylene Compound

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene 1111NX BA4 Polypropylene Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 20% BARIUM SULPHATE REINFORCED HIGH GLOSS APPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 33.8 MPa
4900 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Yield Strength 43.1 MPa
6260 psi
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 0.304 J/cm

@Temperature 23.0 °C
0.569 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648
Users viewing this material also viewed the following: