Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.250 - 0.350 J/cm | 0.468 - 0.656 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8425 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Izod Impact, Notched | 0.220 - 0.350 J/cm | 0.412 - 0.656 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8505Gray20 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Izod Impact, Notched | 0.220 - 0.350 J/cm | 0.412 - 0.656 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8505Gray25 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Izod Impact, Notched | 0.220 - 0.350 J/cm | 0.412 - 0.656 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8505Gray35 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Izod Impact, Notched | 0.220 - 0.350 J/cm | 0.412 - 0.656 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8505Gray40 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Izod Impact, Notched | 0.250 - 0.350 J/cm | 0.468 - 0.656 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8505Gray50 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Izod Impact, Notched | 0.350 - 0.350 J/cm @Temperature -40.0 - -20.0 °C |
0.656 - 0.656 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.350 J/cm Grade Count:1 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 0.300 - 0.350 J/cm | 0.562 - 0.656 ft-lb/in | ASTM D256 |
Loxim 300 00HB Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.250 - 0.350 J/cm | 0.468 - 0.656 ft-lb/in | ASTM D256 |
Loxim 830 02C HB Polypropylene Compound, 30% Calcite Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.300 - 0.350 J/cm | 0.562 - 0.656 ft-lb/in | UV Postcure; ASTM D256A |
DSM Somos® NeXt LV Grey The second member of the Somos® NeXt family, Somos® NeXt LV Grey delivers the durability and functionality, with a finer resolution of details and faster part processing. This third-generation, hi.. |
|||
Izod Impact, Notched | 0.250 - 0.350 J/cm | 0.468 - 0.656 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App.. |
|||
Izod Impact, Notched | 0.220 - 0.350 J/cm | 0.412 - 0.656 ft-lb/in | IS 13411-1992 |
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Good tracking resistanceGood dielectric strengthGood electrical insulation
Applications:Switchgear components which ought to have high tracking resistanceCircuit protecting switche.. |
|||
Izod Impact, Notched | 0.350 - 0.350 J/cm @Temperature -40.0 - -20.0 °C |
0.656 - 0.656 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.350 J/cm Grade Count:1 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |