Mechanical Properties Metric English Comments
Izod Impact, Notched 0.588399 - 0.686465 J/cm

@Temperature -30.0 - -30.0 °C
1.10231 - 1.28603 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.826 J/cm Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Izod Impact, Notched 0.588399 - 0.686465 J/cm

@Thickness 3.17 - 6.35 mm
1.10231 - 1.28603 ft-lb/in

@Thickness 0.125 - 0.250 in
Average value: 0.826 J/cm Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Izod Impact, Notched 0.588399 - 5338.47 J/cm

@Temperature -40.0 - -20.0 °C
1.10231 - 10001.1 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 1.52 J/cm Grade Count:22
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Notched 0.588399 - 5338.47 J/cm

@Thickness 3.17 - 6.40 mm
1.10231 - 10001.1 ft-lb/in

@Thickness 0.125 - 0.252 in
Average value: 1.52 J/cm Grade Count:22
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Notched 0.588399 - 1.49492 J/cm

@Temperature -30.0 - -20.0 °C
1.10231 - 2.80060 ft-lb/in

@Temperature -22.0 - -4.00 °F
Average value: 0.752 J/cm Grade Count:5
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..
Izod Impact, Notched 0.588399 - 1.49492 J/cm

@Thickness 3.17 - 6.40 mm
1.10231 - 2.80060 ft-lb/in

@Thickness 0.125 - 0.252 in
Average value: 0.752 J/cm Grade Count:5
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..